語系:
繁體中文
English
說明(常見問題)
回圖書館首頁
手機版館藏查詢
登入
回首頁
切換:
標籤
|
MARC模式
|
ISBD
Electrospun poly (vinyl alcohol)/ al...
~
Lizu, Monira.
FindBook
Google Book
Amazon
博客來
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers.
紀錄類型:
書目-語言資料,印刷品 : Monograph/item
正題名/作者:
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers./
作者:
Lizu, Monira.
面頁冊數:
61 p.
附註:
Source: Masters Abstracts International, Volume: 52-02.
Contained By:
Masters Abstracts International52-02(E).
標題:
Chemistry, General. -
電子資源:
http://pqdd.sinica.edu.tw/twdaoapp/servlet/advanced?query=1544801
ISBN:
9781303361548
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers.
Lizu, Monira.
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers.
- 61 p.
Source: Masters Abstracts International, Volume: 52-02.
Thesis (M.S.)--Lamar University - Beaumont, 2013.
Poly (vinyl alcohol) (PVA)/alpha-zirconium phosphate (ZrP) polymer nanocomposite (PNC) fibers were successfully prepared via the simple and low-cost electrospinning process. ZrP nanoparticles with two different dimensions, i.e., ZrP-500 with a lateral dimension of ca. 320 nm and an aspect ratio of ca. 500, and ZrP-1500 with a lateral dimension of ca. 950 nm and an aspect ratio of ca. 1500, were utilized to illustrate the size effect on the electrospun nanofibers. In order to obtain defect-free, uniform polymer nanocomposite fibers, a number of parameters including polymer concentration, feed rate, applied voltage and working distance between the needle tip and the fiber collecting substrate were investigated. Scanning electron microscopy (SEM) morphological analysis showed smooth and nonwoven electrospun nanofiber mat. Strong intermolecular interactions between the PVA matrix and the included ZrP nanofillers were revealed by the attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR). The incorporation of ZrP nanofillers drastically improved the thermal stability of the PNC fibers. TGA results demonstrated a clear thermal stability dependence on the aspect ratio of the crystalline ZrP nanofillers. The degradation temperature was increased by 90 °C for the ZrP-1500 and 60 °C for ZrP-500 when the loading level was increased from 1% to 5%. Furthermore, the viscoelastic properties of the PNC solutions were studied by rheometer.
ISBN: 9781303361548Subjects--Topical Terms:
1021807
Chemistry, General.
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers.
LDR
:02327nam a2200277 4500
001
1960694
005
20140624205951.5
008
150210s2013 ||||||||||||||||| ||eng d
020
$a
9781303361548
035
$a
(MiAaPQ)AAI1544801
035
$a
AAI1544801
040
$a
MiAaPQ
$c
MiAaPQ
100
1
$a
Lizu, Monira.
$3
2096399
245
1 0
$a
Electrospun poly (vinyl alcohol)/ alpha-zirconium phosphate nanocomposite fibers.
300
$a
61 p.
500
$a
Source: Masters Abstracts International, Volume: 52-02.
500
$a
Adviser: Suying Wei.
502
$a
Thesis (M.S.)--Lamar University - Beaumont, 2013.
520
$a
Poly (vinyl alcohol) (PVA)/alpha-zirconium phosphate (ZrP) polymer nanocomposite (PNC) fibers were successfully prepared via the simple and low-cost electrospinning process. ZrP nanoparticles with two different dimensions, i.e., ZrP-500 with a lateral dimension of ca. 320 nm and an aspect ratio of ca. 500, and ZrP-1500 with a lateral dimension of ca. 950 nm and an aspect ratio of ca. 1500, were utilized to illustrate the size effect on the electrospun nanofibers. In order to obtain defect-free, uniform polymer nanocomposite fibers, a number of parameters including polymer concentration, feed rate, applied voltage and working distance between the needle tip and the fiber collecting substrate were investigated. Scanning electron microscopy (SEM) morphological analysis showed smooth and nonwoven electrospun nanofiber mat. Strong intermolecular interactions between the PVA matrix and the included ZrP nanofillers were revealed by the attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR). The incorporation of ZrP nanofillers drastically improved the thermal stability of the PNC fibers. TGA results demonstrated a clear thermal stability dependence on the aspect ratio of the crystalline ZrP nanofillers. The degradation temperature was increased by 90 °C for the ZrP-1500 and 60 °C for ZrP-500 when the loading level was increased from 1% to 5%. Furthermore, the viscoelastic properties of the PNC solutions were studied by rheometer.
590
$a
School code: 0424.
650
4
$a
Chemistry, General.
$3
1021807
650
4
$a
Nanoscience.
$3
587832
690
$a
0485
690
$a
0565
710
2
$a
Lamar University - Beaumont.
$b
Chemistry and Biochemistry.
$3
2096400
773
0
$t
Masters Abstracts International
$g
52-02(E).
790
$a
0424
791
$a
M.S.
792
$a
2013
793
$a
English
856
4 0
$u
http://pqdd.sinica.edu.tw/twdaoapp/servlet/advanced?query=1544801
筆 0 讀者評論
館藏地:
全部
電子資源
出版年:
卷號:
館藏
1 筆 • 頁數 1 •
1
條碼號
典藏地名稱
館藏流通類別
資料類型
索書號
使用類型
借閱狀態
預約狀態
備註欄
附件
W9255522
電子資源
11.線上閱覽_V
電子書
EB
一般使用(Normal)
在架
0
1 筆 • 頁數 1 •
1
多媒體
評論
新增評論
分享你的心得
Export
取書館
處理中
...
變更密碼
登入